Effects of Water, Alcohols Impurities in Polyaspartic Flooring Formulation The influence of water and small molecular alcohols on the reaction rate is remarkable A Solvent water content and purity B Powder water content C Dilute solvents for additives such as leveling agent, defoaming agent, etc. Wa... View More
➤ Visit Website
![China Spraying Polyaspartic Weather Resistance Coating Formulation Pull-out Testing Problem for sale](http://img1.tradegrowthhub.com/89/1f/f0747e55f4f9/product/12156214_s-w400xh400.jpg)
Spraying Polyaspartic Weather Resistance Coating Formulation Pull-out Testing Problem
Price: Negotiable
MOQ: 200KG
Delivery Time: 7 days after getting order
Brand: Feiyang Novel Materials
Problem: pull-out test brush is OK, but spraying film failed, only 3-4Mpa, polyaspartic topcoat film delaminate level by level when doing pull-out test. Request Date: Pull-out Testing above 7.5Mpa. Background: 1. metal substrate 2. Polyaspartc topcoat on polyurethane 3. Machine spraying. Problem: pu... View More